Material | Grade | Br | Hcb | Hcj | (BH)max | Tc | Tw | Br α(Br) | Hcj β(Hcj) | ||||
T | KGs | KA/m | Koe | KA/m | Koe | KJ/m3 | MGOe | ℃ | ℃ | %/℃ | %/℃ | ||
SmCo5 | YX-16s | 0.79-0.84 | 7.9-8.4 | 620-660 | 7.8-8.3 | ≥1830 | ≥23 | 118-135 | 15-17 | 750 | 250 | -0.035 | -0.28 |
YX-18s | 0.84-0.89 | 8.4-8.9 | 660-700 | 8.3-8.8 | ≥1830 | ≥23 | 135-151 | 17-19 | 750 | 250 | -0.04 | -0.28 | |
YX-20s | 0.89-0.93 | 8.9-9.3 | 684-732 | 8.6-9.2 | ≥1830 | ≥23 | 150-167 | 19-21 | 750 | 250 | -0.045 | -0.28 | |
YX-22s | 0.92-0.96 | 9.2-9.6 | 710-756 | 8.9-9.5 | ≥1830 | ≥23 | 167-183 | 21-23 | 750 | 250 | -0.045 | -0.28 | |
YX-24s | 0.96-1.00 | 9.6-10.0 | 740-788 | 9.3-9.9 | ≥1830 | ≥23 | 183-199 | 23-25 | 750 | 250 | -0.045 | -0.28 | |
Low Temperature Coefficient 1:5 (SmGd)Co5 | T | 0.62-0.66 | 6.2-6.6 | 485-517 | 6.1-6.5 | ≥1830 | ≥23 | 75-88 | 9.5-11 | 750 | 250 | 20-100℃ 100-200℃ 200-300℃ | Br +0.0156%/℃ +0.0087%/℃ +0.0007%/℃ |
Material | Grade | Br | Hcb | Hcj | (BH)max | Tc | Tw | Br α(Br) | Hcj β(Hcj) | ||||
T | KGs | KA/m | Koe | KA/m | Koe | KJ/m3 | MGOe | ℃ | ℃ | %/℃ | %/℃ | ||
SmCo2:17 | YXG-24H | 0.95-1.02 | 9.5-10.2 | 692-764 | 8.7-9.6 | ≥1990 | ≥25 | 175-191 | 22-24 | 800 | 350 | -0.035 | -0.2 |
Sm2 | YXG-26H | 1.02-1.05 | 10.2-10.5 | 748-796 | 9.4-10.0 | ≥1991 | ≥25 | 191-207 | 24-26 | 800 | 350 | -0.035 | -0.2 |
(CoFeCuZr)17 | YXG-26M | 1.02-1.05 | 1.02-1.05 | 676-780 | 8.5-9.8 | 955-1433 | 12--18 | 199-215 | 25-27 | 800 | 300 | -0.035 | -0.2 |
YXG-32M | 1.10-1.13 | 11.0-11.3 | 676-852 | 8.5-10.7 | 955-1433 | 12--18 | 230-255 | 29-32 | 800 | 300 | -0.035 | -0.2 | |
YXG-30L | 1.08-1.15 | 10.8-11.5 | 541-796 | 6.8-10.0 | 636-955 | 8--12 | 220-240 | 28-30 | 800 | 250 | -0.035 | -0.2 | |
Low Temperature Coefficient 1:5 | LTC(YXG-18) | 0.84-0.89 | 8.4-8.9 | 629-668 | 7.9-8.4 | ≥1433 | ≥18 | 135-151 | 17-19 | 840 | 300 | -0.001 | -0.25 |
(SmGd)Co17 | LTC(YXG-20) | 0.89-0.94 | 8.9-9.4 | 660-708 | 8.3-8.9 | ≥1433 | ≥18 | 151-167 | 19-21 | 840 | 300 | -0.007 | -0.25 |
LTC(YXG-22) | 0.94-0.98 | 9.4-9.8 | 692-740 | 8.7-9.3 | ≥1433 | ≥18 | 167-183 | 21-23 | 840 | 300 | 0.001 | -0.25 | |
High Temperature | HT400(YXG-26) | 0.99-1.04 | 9.9-10.4 | 740-812 | 9.3-10.2 | ≥1830 | ≥23 | 191-215 | 24-27 | 850 | 400 | -0.035 | -0.12 |
Sm2 | HT450(YXG-24) | 0.96-0.99 | 9.6-9.9 | 724-772 | 9.1-9.7 | ≥1830 | ≥23 | 175-199 | 22-25 | 850 | 450 | -0.035 | -0.12 |
(CoFeCuZr)17 | HT500(YXG-22) | 0.93-0.97 | 9.3-9.7 | 708-756 | 8.9-9.5 | ≥1830 | ≥23 | 160-183 | 20-23 | 850 | 500 | -0.035 | -0.12 |
Materials | SmCo5 | Sm2Co17 | Controlled Coercivity Sm2Co17 | Temperature Compensation Magnet Sm2Co1 | |||||||
Grade | GSM-22 | GSM-24H | GSM-26H | GSM-28H | GSM-30H | GSM-32H | GSM-30L | GSM-32L | GSM-18D | GSM-20D | GSM-22D |
Br(T) | 0.90-1.00 | 0.94-1.04 | 0.98-1.08 | 1.02-1.12 | 1.06-1.16 | 1.08-1.18 | 1.06-1.16 | 1.08-1.16 | 0.80-0.90 | 0.85-0.95 | 0.90-1.00 |
Residual Induction | (9.0-10.0) | (9.4-10.4) | (9.8-10.8) | (10.2-11.2) | (10.6-11.6) | (10.8-11.8) | (10.6-11.6) | (10.8-11.6) | (8.0-9.0) | (8.5-9.5) | (9.0-10.0) |
Hcb(KA/m) | 677-780 | 709-748 | 733-772 | 749-827 | 773-883 | 804-883 | 319-716 | 319-716 | 558-676 | 597-716 | 637-756 |
Coercive Force(Koe) | (8.5-9.8) | (8.9-9.4) | (9.2-9.7) | (9.4-10.4) | (9.7-11.1) | (10.1-11.1) | (4.0-9.0) | (4.0-9.0) | (7.0-8.5) | (7.5-9.0) | (8.0-9.5) |
Hcj(KA/m) | ≥1433 | ≥1592 | ≥1592 | ≥1592 | ≥1592 | ≥1592 | 558-1592 | 558-1592 | ≥1433 | ≥1592 | ≥1592 |
Intrinsic Coercive Force(Koe) | (≥18) | (≥20) | (≥20) | (≥20) | (≥20) | (≥20) | (7.0-20.0) | (7.0-20.0) | (≥18) | (≥20) | (≥20) |
(BH)max(KJ/m 3) Max. Energy Product(MGOe) | 159-191 | 175-207 | 191-223 | 207-239 | 223-255 | 231-263 | 223-255 | 231-263 | 127-159 | 143-175 | 159-191 |
(20-24) | (22-26) | (24-28) | (26-30) | (28-32) | (29-33) | (28-32) | (29-33) | (16-20) | (18-22) | (20-24) | |
αBr(%/℃) | -0.065 | -0.03 | -0.036 | -0.041 | -0.04 | -0.04 | -0.044 | 800-850 | 0.045 | 0.004 | 0.001 |
Thermal Coefficient of Br | *(1) | *(1) | *(1) | ||||||||
Max.Operating Temperature(℃) | 250 | 350 | 350 | 350 | 350 | 350 | 350 | 350 | 350 | 350 | 350 |
Tc Curie Point (℃) | 700-750 | 800-850 | |||||||||
ρDensity (kg/m³) | 8.1-8.4×103 | 8.2-8.5×103 |
In the aerospace industry, where components are exposed to extreme conditions. Ketian's SmCo disc magnets provide precise and durable solutions, ensuring actuators and navigation systems operate reliably in high-altitude environments.
In medical applications, including MRI machines and prosthetic components, Ketian's custom made neodymium magnets ensure long-term reliability and precision in sensitive medical devices, making them the preferred choice for healthcare providers.
For the automotive industry, SmCo magnets are used in electric motors and anti-lock braking systems, where their ability to withstand high temperatures and maintain strength over time is crucial. As a leading samarium cobalt magnet manufacturer, Ketian offers SmCo disc magnets and other forms with exceptional durability, meeting the demanding standards of modern vehicles.
In industrial machinery, renewable energy, and sensor systems, Ketian's SmCo magnets provide the robustness required for high-performance motors, wind turbines, and position sensors, ensuring optimal efficiency and long-term operation even in harsh environments.
High-Quality SmCo Magnets
Ketian is a trusted Samarium Cobalt magnet manufacturer, known for producing top-tier SmCo magnets that offer exceptional properties like high-temperature stability, corrosion resistance, and superior magnetic strength.
Customization to Meet Specific Needs
As a leading Samarium Cobalt magnet supplier, Ketian understands that every application has unique requirements. We offer custom SmCo disc magnets in various shapes, sizes, and grades to ensure the perfect fit for your project.
Durability and Long-Lasting Performance
Our SmCo magnets are engineered for durability and longevity. With a high resistance to demagnetization, SmCo magnets from Ketian perform reliably in extreme temperatures and harsh environments.
Cost-Effective Solutions
While Samarium Cobalt magnets are often more expensive than other types of magnets, Ketian ensures you receive a high value for your investment by providing affordable pricing without compromising on quality. We work directly with clients to deliver SmCo disc magnets and other magnet types that meet both performance needs and budget constraints.
Industry Expertise
With years of experience as a Samarium Cobalt magnet manufacturer, Ketian has developed deep expertise in magnet production and application. We provide not only superior products but also expert consultation to help you choose the best Samarium Cobalt magnets for your specific requirements.
Global Reach and Reliable Delivery
As one of well-established NdFeB magnets manufacturers, Ketian serves clients worldwide. We ensure quick, efficient delivery of SmCo magnets and maintain excellent communication to meet your timeline. Our global logistics network guarantees that your order of SmCo disc magnets will arrive on time and in perfect condition.